Mineral: |
Goethite |
Reference: |
S04d |
SCM Type: |
DDL - Diffuse Double Layer |
Ligand: |
Zn<2+>
- zinc
|
Site Type: |
»Fe(s)-OH |
Equation: |
»Fe(s)-OH + Zn<2+> + SO4<2-> ⇔ »Fe(s)-OH-ZnSO4 |
LogK: |
9.0 ± 0.027
LogK°I=0 (Conversion to I = 0): 9.00
LogK2.31 nm−2 (SSD-normalized): 8.03
|
Experiment: |
Batch Sorption Experiments |
Ionic Strength: |
0.0 mol/L
|
Temperature: |
298.15 K |
pH Range: |
4 - 7 |
Fit Method: |
FITEQL |
Comment: |
Zn concentration of 2.95 µmol/kg,
SO4 concentration of 5.02 mmol/kg;
1.48 g/kg Goethite |
|