Surface Complex Formation Data:

Mineral: Ferrihydrite
Reference: SWM03
SCM Type: DDL - Diffuse Double Layer
Ligand: Cd<2+> - cadmium
Site Type: »Fe(w)-OH
Equation: »Fe(w)-OH + Cd<2+> + SO4<2->  ⇔  »Fe(w)-OH-CdSO4
LogK: 6.51 ± 0.08         LogK°I=0 (Conversion to I = 0):   6.51         LogK2.31 nm−2 (SSD-normalized):   8.71
Experiment: Batch Sorption Experiments
Ionic Strength: 0.0 mol/L
Temperature: 298.15 K
pH Range: 5 - 8
Fit Method: FITEQL
Comment: Cd conc. of 9.67 µmol/kg, Fe concentration of 10.5 mmol/kg, SO4 concentration of 2.01 mmol/kg
 