RES³T - Rossendorf Expert System for Surface and Sorption Thermodynamics

Show Detailed Site Query Results


Binding Site Data:


Mineral: Hematite
Reference: SVYT03
SCM Type: TL - Triple Layer   (C1: 1.1 F/m2,  C2: 0.05 F/m2)
Ionic Strength: 0.001 mol/L of NaNO3
Site Type: »Fe-OH
PZC:
pK1: 2.98 pK1°I=0 (Conversion to I = 0): 2.96 pK12.31 nm−2 (normalized): 3.49
pK2: 2.46 pK2°I=0 (Conversion to I = 0): 2.44 pK22.31 nm−2 (normalized): 1.95
Site Density in nm-2: 7.5000
Original Site Density: 7.5 sites / nm² surface
Solid/Liquid Ratio in g/L: 10.0
pH Range: 2-10
Temperature in K: 298.0
Method for Site Density: Mean of Different Sources
Method for Protolysis:Batch Sorption Experiments
Fit Method:KINEQL
Comment: unspecified: ferric oxide; tempearture 25+-1°C; SSD based on typically literature values
 
1 data sets were retrieved