Mineral: |
Spherocobaltite |
Reference: |
PS02b |
SCM Type: |
CC - Constant Capacitance
(C1: 31.0 F/m2) |
Ionic Strength: |
0.0 mol/L of
NaCl
|
Site Type: |
»CO3H |
PZC: |
5.75 |
pK1: |
|
pK1°I=0 (Conversion to I = 0): |
|
|
pK2: |
5.0 |
pK2°I=0 (Conversion to I = 0): |
5.00 |
pK22.31 nm−2 (normalized): |
4.60 |
Site Density in nm-2: |
5.8534 |
Original Site Density: |
9.72 µmol / m² surface
|
Solid/Liquid Ratio in g/L: |
|
pH Range: |
|
Temperature in K: |
298.15 |
Method for Site Density: |
Geometrical Calculation |
Method for Protolysis: | Electrophoretic Mobility |
Fit Method: | MINTEQA2 |
Comment: |
PZC at 0.005 M sumCO2; temperature 25+-1°C |
|
Mineral: |
Spherocobaltite |
Reference: |
PS02b |
SCM Type: |
CC - Constant Capacitance
(C1: 31.0 F/m2) |
Ionic Strength: |
0.0 mol/L of
NaCl
|
Site Type: |
»Co-OH |
PZC: |
5.75 |
pK1: |
9.2 |
pK1°I=0 (Conversion to I = 0): |
9.20 |
pK12.31 nm−2 (normalized): |
9.60 |
pK2: |
13.0 |
pK2°I=0 (Conversion to I = 0): |
13.00 |
pK22.31 nm−2 (normalized): |
12.60 |
Site Density in nm-2: |
5.8534 |
Original Site Density: |
9.72 µmol / m² surface
|
Solid/Liquid Ratio in g/L: |
|
pH Range: |
|
Temperature in K: |
298.15 |
Method for Site Density: |
Geometrical Calculation |
Method for Protolysis: | Electrophoretic Mobility |
Fit Method: | MINTEQA2 |
Comment: |
PZC at 0.005 M sumCO2; temperature 25+-1°C |
|