Mineral: Birnessite
Reference: VFCBG16
Preparation: synthesized by adding 35% HCl dropwise to a boiling solution of 0.4 M KMnO4 under vigorous stirring [31]; filtered, washed with 300 mL of distilled water 4–5 times, air-dried, and then ground and stored for further analyses
CEC: 158.55 ± 0.662 meq/100g
Sample characterized via: ☑ X-ray photoelectron spectroscopy (XPS)
☑ FT-IR spectroscopy
☑ Scanning electron microscope (SEM)
☑ X-ray Diffraction (XRD)
 