RES³T - Rossendorf Expert System for Surface and Sorption Thermodynamics

Details Sample Characterization



Mineral: Goethite
Reference: RZEAA88
Trade Name: M-Al
Preparation: acc. to Goodman and Lewis, 1981: 0.035M FeCl2/0.015M AlCl3 solution mixed with NaCO3 to pH7, suspension aerated until oxidation was complete (7d), dialyzed 14d, freeze-dried, stored in desiccator
Composition: 21.9 mol% Al-substitution; sample M-Al
Sample characterized via: ☑ X-ray Diffraction (XRD)
 
1 data sets were retrieved