RES³T - Rossendorf Expert System for Surface and Sorption Thermodynamics

Details Sample Characterization



Mineral: Baddeleyite (Zirconia)
Reference: EVPBL19
Supplier: ChemPUR
Preparation: heat-treated by means of calcination for 5 h at 1000 °C under ambient atmosphere in a ceramic crucible; heating rate of 200 °C/h; after the completed calcination time, the oven was switched off and left to cool; calcined product was ground using an agate mortar and pestle
Crystallinity: monoclinic
Dimension: crystallite size: ~45 nm, agglomerate size: 13 ± 6 µm
Sample characterized via: ☑ Scanning electron microscope (SEM)
☑ X-ray Diffraction (XRD)
Comment: Total Carbon content = 0.13 ± 0.03 mg/g
 
1 data sets were retrieved