Mineral: Montmorillonite
Reference: PKKDR18
Supplier: Sigma
Trade Name: K-10 (Montmorillonite clay)
Preparation: dispersed in 1 M NaCl for 24 h (cleaned and converted into homoionic Na-form), clay was separated by centrifugation, twice rinsed with Milli Q water, clay was separated by centrifugation, drying at 100°C in vacuum oven
CEC: 23.0 ± 0.0 meq/100g
Composition: 67.1 wt% SiO2, 11.6 wt% Al2O3, 1.4 wt% MgO, 1.85 Na2O, 1.4 wt% K2O, 15.8 wt% Fe2O3, 0.07 wt% CaO, 0.55 wt% TiO2
Sample characterized via: ☑ FT-IR spectroscopy
☑ Scanning electron microscope (SEM)
☑ X-ray Diffraction (XRD)
 
1 data sets were retrieved