Preparation: hydrolysis of FeCl3 from a homogeneous solution containing equal volumes of 0.037M FeCl3 and 0.75M urea under reflux for 45min, precipitate washed, dried at room temperature
Crystallinity: well crystallized; TEM: spindle or wheat-grain-shaped paticles
Composition: total iron content 58.1%, empirical formula FeOOH*0.3 H2O, 1.9% Cl-; TGA: 14.5% H2O
Sample characterized via: ☑ Transmission electron microscopy (TEM)
☑ X-ray Diffraction (XRD)
 