Mineral: |
Goethite |
Reference: |
SWM09 |
SCM Type: |
DDL - Diffuse Double Layer |
Ligand: |
Cd<2+>
- cadmium
|
Site Type: |
»Fe(s)-OH |
Equation: |
»Fe(s)-OH + Cd<2+> + SO4<2-> ⇔ »Fe(s)-OH-CdSO4 |
LogK: |
9.63 ± 0.031
LogK°I=0 (Conversion to I = 0): 9.63
LogK2.31 nm−2 (SSD-normalized): 8.66
|
Experiment: |
Batch Sorption Experiments |
Ionic Strength: |
0.0 mol/L
|
Temperature: |
298.15 K |
pH Range: |
5 - 8 |
Fit Method: |
FITEQL |
Comment: |
Cd concentration of 1.62 µmol/kg,
SO4 concentration of 2.12 mmol/kg;
1.34 g/kg Goethite |
|