Mineral: |
Hematite |
Reference: |
KILL99 |
SCM Type: |
ECC - Extended Constant Capacitance |
Ligand: |
Sr<2+>
- strontium
|
Site Type: |
»Fe-OH |
Equation: |
»Fe-OH + Sr<2+> + H2O ⇔ »Fe-O-Sr(OH) + 2 H<1+> |
LogK: |
-14.15 ± 0.02
LogK°I=0 (Conversion to I = 0): -13.94
LogK2.31 nm−2 (SSD-normalized): -13.21
|
Experiment: |
Batch Sorption Experiments |
Ionic Strength: |
0.1 mol/L
NaCl
|
Temperature: |
348.15 K |
Solid/Liquid Ratio: |
70.0 g/L |
pH Range: |
7.8-10.0 |
Ligand Concentration Range: |
2E-4. 1E-3. 2E-3 mol/L |
Fit Method: |
FITEQL |
Comment: |
moreover, datasets for 25°C and 50 °C are reported. |
|