Mineral: |
Baddeleyite (Zirconia) |
Reference: |
EVPBL19 |
SCM Type: |
DDL - Diffuse Double Layer
|
Ionic Strength: |
0.0 mol/L of
|
Site Type: |
»Zr-OH |
PZC: |
|
pK1: |
4.0 |
pK1°I=0 (Conversion to I = 0): |
4.00 |
pK12.31 nm−2 (normalized): |
4.51 |
pK2: |
8.1 |
pK2°I=0 (Conversion to I = 0): |
8.10 |
pK22.31 nm−2 (normalized): |
7.59 |
Site Density in nm-2: |
7.5600 |
Original Site Density: |
7.56 sites / nm² surface
|
Solid/Liquid Ratio in g/L: |
|
pH Range: |
|
Temperature in K: |
|
Method for Site Density: |
Geometrical Calculation |
Method for Protolysis: | Literature |
Fit Method: |
Comment: |
SSD of ZrO2 was calculated using a crystallographic approach; surface protolysis reactions taken from Blackwell and Carr 1991 (ref. [60] in the article) |
|