Mineral: |
Bentonite |
Reference: |
SXWFW09 |
SCM Type: |
DDL - Diffuse Double Layer
|
Ionic Strength: |
0.01 mol/L of
NaClO4
|
Site Type: |
»X-OH |
PZC: |
|
pK1: |
|
pK1°I=0 (Conversion to I = 0): |
|
|
pK2: |
6.361 |
pK2°I=0 (Conversion to I = 0): |
6.32 |
pK22.31 nm−2 (normalized): |
6.02 |
Site Density in nm-2: |
5.0585 |
Original Site Density: |
0.000252 mol / g solid
|
Solid/Liquid Ratio in g/L: |
5.4 |
pH Range: |
3 - 11 |
Temperature in K: |
298.15 |
Method for Site Density: |
Potentiometric Titration |
Method for Protolysis: | Potentiometric Titration |
Fit Method: | FITEQL |
Comment: |
SSA not given in this study, taken from [MAG06] (also SUBATECH MX-80 Bentonite) |
|